* The product must be capable of with standing the severe tests described. abobe,and in addition the coating must not soften or weaken in the least even at a temperature of approx 300
* One month after a hig-temperature cathodic disbonding testi93APH12jthe disbonded area was approx. 0.5u. Showing excellent results which would have been un-thinkable with conventional anti corrosives applied on site.
* Even at higt temperatures,the products prevent the entry of water, Which is the cause of rust.
* Much as with conventional single-liquid air-drying coatings,the products are applied without heating and in a short time. It is possible to complete application in one day even for a coating thickness of nearly 1,500.
* BTX DRAIN-PIPES LAID UNDER THE GROUND
* FUEL PIPES FOR OIL HEAT POWER
* MUFFLER OF DIESEL ENGINE FOR GENERATION OF ELECTRIC POWER
* STEEM PIPES FOR VESSEL
* DIDES FOR AIR-COOLING AND HEATING
* HEAT EXCHANGER
* PIPES HIGH TEMPERATURE DUCT
|